Objective
Composites of fluoropolymers and low-density metals (e.g., aluminum and magnesium) are highly attractive energetic materials due to their high volumetric and gravimetric energy release upon combustion, but they also pose significant safety hazards if disposed improperly. For example, the composites can detonate upon ignition caused by heat or impact. Therefore, the proper separation and hazard elimination of fluoropolymer-metal composites is of great relevance and importance to the Department of War (DoW).
The objective of this proof-of-concept project is to formulate a novel process that can transform the fluoropolymer-metal composites into two separate phases with low hazard levels: the fluoropolymer with <1 wt.% metal impurities, and a neutral aqueous solution containing the metal ions. The project will employ efficient and easy-to-use methods (e.g., cryogenic grinding and filtration) and low impact chemicals (e.g., water and sodium chloride), ensuring that the method is easy to scale and cost-effective.
Technical Approach
The overarching hypothesis of this project is that cryogenic temperatures make Teflon and Viton polymers brittle, thus increasing their susceptibility to fracture under mechanical force. As a result, ball milling at cryogenic temperatures will allow the liberation and the following separation of metal particles from their composites with Teflon or Viton. As illustrated in the figure below, the key to the separation of fluoropolymer-metal composites lies in developing a methodology that can disrupt the polymer matrix and expose the metal particles for the following separation process. Cryogenic grinding under liquid nitrogen temperature is well suited for this purpose because it works at temperatures far below the glass transition temperatures of polymers. After cryogenic grinding, the metal particles (e.g., aluminum) will be converted to aqueous ionic species (e.g., aluminum or aluminate ions) by reacting with water. The effect of additives such as sodium chloride, sodium nitrate, and low concentrations (e.g., <1 mM) of acids or bases will be evaluated since they can effectively produce localized pitting and rupture of the protective layer on aluminum or magnesium particles and promote their reaction with water. Finally, the fluoropolymer powders will be separated from the aqueous solution via filtration. The methodology will be validated using two model composites: Teflon-aluminum and Viton-aluminum. Since Teflon is not soluble in most solvents, its composite with aluminum will be prepared by mechanical milling commercially available micron-sized particles of Teflon and aluminum. The Viton-aluminum composite with a metal-polymer core-shell structure will be prepared by coating aluminum particles with Viton from a solution. Aluminum has been selected over magnesium in this project because the dissolution of aluminum is technically more challenging than magnesium.

Benefits
Commercial cryogenic grinding equipment can provide batch sizes up to 7 kilograms, and the cost of liquid nitrogen can be as low as $0.13 per liter if produced on site. The method generates products with reduced hazard classification which will provide a lower disposal cost for DoW. (Anticipated Project Completion - 2027)